Atmospheres for conditioning and testing — Determination of relative humidity — Part 2: Whirling psy...
The method specified applies for temperatures within the range from 5 to 80 °C. The property is determined with an uncertainty not exceeding 3 % r. h. The method is restricted to wet-bulb temperatures not lower than 1 C, dry-bulb temperatures not higher than 80 °C, and pressures not differing from standard atmospheric pressure by more than 30 %.
Wrought aluminium and aluminium alloy sheets, strips and plates — Part 3: Strips — Tolerances on sha...
This part of ISO 6361 specifies to strips for thicknesses up to and including 6,3 mm in accordance with the definition in ISO 3134-3, tolerances on thickness, width and lateral curvature.
The purpose of the measuring method is to determine the residual camber height and length as a function of the load ("flattening test"). Gives some essential informations related to the parameters "contact load" and "standard camber length". Applies to cross-country skis of size 130 cm and longer.
Specifies a method for estimating the water distribution in relation to a grading scale which is enclosed to the standard. The water dispersion value of butter is used for grading purposes because the size and distribution of the water droplets is applicable to all types of butter. The sampling shall be made in accordance with ISO 707.
Atmospheres for conditioning and testing — Determination of relative humidity — Part 1: Aspirated ps...
The method specified applies for temperatures within the range from 5 to 80 °C. The property is determined with an uncertainty either not exceeding 3 % r. h. or not exceeding 3 % r. h., depending on the uncertainty in the value obtained for the wet-bulb temperature depression and on whether or not the dry-bulb temperature exceeds 40 °C.
Ductile iron pipes for pressure and non-pressure pipelines — Centrifugal cement mortar lining — Gene...
This second edition cancels and replaces the first edition (1980). Specifies the nature, the method of application, the surface condition and the minimum thickness of internal linings for pipes as defined in ISO 2531 and ISO 7186. Tabulates nominal sizes from DN 40 up to and including DN 2600.
Beurre — Détermination de l'indice de dispersion de l'eau
La présente Norme internationale spécifie une méthode pour la détermination de l'indice de dispersion de l'eau dans le beurre.
NOTE -- L'indice de dispersion de l'eau dans le beurre est utilisé à des fins de classement, car la taille et la répartition des gouttelettes d'eau sont étroitement liées à la durée de conservation du beurre. La méthode est applicable à tous les…
Skis de fond — Détermination des performances dynamiques — Méthode de mesurage en laboratoire
La présente Norme internationale spécifie une méthode
de détermination des performances dynamiques des skis de fond. Le but
de cet essai est de déterminer la hauteur et la longueur de cambre résiduel
en fonction de la charge. Une autre appellation pour cet essai est : «essai
de mise à plat». Les diagrammes (pour les exemples voir les figures
2 et 3) obtenus selon cet essai sont…